Posted in

What are the common failures of titanium equipment and how to prevent them?

If you’ve worked with industrial processing equipment—whether for chemical manufacturing, pharmaceutical production, food and beverage processing, or aerospace component fabrication—you know titanium stands out as a go-to material. Its high strength-to-weight ratio, exceptional corrosion resistance, and ability to perform reliably in extreme temperatures make it irreplaceable for so many applications. But titanium isn’t invincible. Even the most well-engineered titanium equipment can fail prematurely, leading to costly downtime, product contamination, and safety risks. Over 12 years as a titanium equipment supplier, I’ve seen every type of failure imaginable, from tiny, hard-to-spot flaws in heat exchangers to catastrophic leaks in reactors. Today, I’m breaking down the most common titanium equipment failures, why they happen, and how we work with clients to prevent them before they cause problems. Titanium Equipment

First, let’s ground this in a quick truth: titanium’s reputation for durability doesn’t come from being indestructible—it comes from its self-healing oxide layer. When titanium is exposed to oxygen (even in trace amounts), it forms a thin, dense TiO₂ layer that adheres tightly to the metal, blocking corrosive agents from penetrating the underlying material. This works flawlessly in neutral or oxidizing environments, but break that layer, and the metal’s vulnerability spikes. Most failures trace back to damage to this passive layer or manufacturing/installation oversights that create weak points.

The most prevalent failure I see across all industries is crevice corrosion, and it’s often the hardest to catch during routine inspections. Crevice corrosion happens in narrow, stagnant gaps between titanium components or between titanium and another material, like a carbon steel flange or a bolt made of a dissimilar metal. Those gaps trap moisture, corrosive chemicals, or debris, creating an oxygen-depleted environment that eats away at the passive layer. For example, a client of ours in the fertilizer industry had a heat exchanger with titanium tubes mated to carbon steel tube sheets. The small gap between the two metals built up stagnant ammonium nitrate solution, leading to crevice corrosion that ate through a tube wall in just 18 months of operation. At first, we thought it was a material defect, but a closer look revealed the root cause: the gaps weren’t sealed properly during assembly, so corrosive fluid seeped in.

How do we prevent this? It starts with design, not just post-installation fixes. Our team works closely with clients to eliminate crevices wherever possible. For joints that can’t be eliminated, we use two key strategies: first, gap fillers made of materials that match titanium’s corrosion properties, like polytetrafluoroethylene (PTFE) gaskets with precise, uniform thickness to avoid uneven gaps. Second, we specify full-contact welding for joints instead of threaded or bolted connections that leave tiny gaps. For the fertilizer client, we retrofitted the tube sheets with titanium cladding and used full-penetration welds to seal tube-to-sheet joints, plus added a periodic flushing protocol for the heat exchanger to prevent stagnant fluid buildup. We also include a pre-installation gap inspection as part of our standard service, checking every joint with a feeler gauge to ensure gaps are within safe limits.

Next, pitting corrosion is another common culprit, especially in industries using chlorides like pharmaceutical manufacturing or desalination. Pitting corrosion is localized, small-scale damage to the passive layer that forms tiny holes in the titanium surface. It’s tricky because these pits are often too small to detect during visual inspections until they’ve grown large enough to cause leaks. Chloride ions (from salt, bleach, or process solutions) are the main trigger here—they are small enough to penetrate the passive layer, especially if there are surface defects from manufacturing, handling, or even improper cleaning.

A client in the biotech sector learned this the hard way a few years ago. They had a titanium storage tank for a sterile buffer solution, and after 2 years, we found small pits on the inner wall near a drain. The buffer solution had trace amounts of sodium chloride, and during initial installation, the tank’s inner surface had a small scratch from a tool used during assembly. That scratch broke the passive layer, and chloride ions targeted the weak spot, causing pitting.

Prevention here hinges on three things: surface quality, process monitoring, and material selection. First, we always perform a surface roughness test on all titanium components before shipment, ensuring Ra values are below 0.8 micrometers—smoother surfaces are less likely to trap corrosive ions or develop defects. We also use only certified titanium billets from trusted mills, with traceable material composition to avoid low-purity titanium that’s more prone to corrosion. For the biotech client, we removed the scratched section of the tank, polished the entire inner wall to a mirror finish, and added a continuous chloride level monitor to their process, alerting operators if concentrations exceed safe limits (we recommend keeping chlorides below 100 ppm for most titanium applications). We also updated their cleaning protocol to use non-chlorinated detergents, eliminating a secondary source of pitting.

Another failure that’s often overlooked is stress corrosion cracking (SCC). This happens when titanium is under mechanical stress (from installation, pressure, or thermal expansion) and is exposed to a specific corrosive environment. For titanium, the worst offenders are high-temperature chloride solutions or certain organic acids, like formic acid. Unlike other failures, SCC develops slowly over months or years, often with no visible signs until a crack forms suddenly, leading to catastrophic equipment failure. A power generation client we worked with had a titanium condenser tube that failed unexpectedly after 3 years. Inspection revealed a crack along a weld seam, caused by residual stress from the welding process and exposure to trace chlorides in the cooling water. The weld had not been properly stress-relieved, leaving internal stress that, combined with the corrosive cooling water, created perfect conditions for SCC.

Preventing SCC requires addressing both stress and environment. First, all titanium components that are welded or formed (like condenser tubes, reactor vessels, or heat exchanger shells) undergo a stress relief heat treatment at 600–700°C (1112–1292°F) after fabrication. This eliminates residual stress from manufacturing. For clients working with high-chloride environments, we also offer alternative titanium alloys—like Ti-6Al-4V ELI, or even more corrosion-resistant Ti-3Al-2.5V—instead of pure titanium. For the power generation client, we heat-treated all their condenser tubes, adjusted their cooling water treatment to reduce chloride levels, and added non-destructive testing (NDT) like ultrasonic testing and eddy current testing during annual maintenance to detect early signs of cracking.

One last common failure is hydrogen embrittlement, which is especially risky in industries like electroplating, metal finishing, and oil and gas. Hydrogen embrittlement happens when hydrogen atoms penetrate the titanium’s crystal structure, making it brittle and prone to cracking under stress. Hydrogen can come from process solutions (like acidic plating baths), welding (if shielding gas is contaminated), or even corrosion reactions. A plating company client had a titanium anode basket that fractured mid-use, ruining a batch of parts and requiring a full shutdown. Testing showed hydrogen had seeped into the titanium during the plating process, where sulfuric acid used in their baths released hydrogen.

Preventing hydrogen embrittlement is all about controlling hydrogen exposure. We add a special process to all titanium components for clients working with acidic environments: after fabrication, we perform a dehydrogenation heat treatment at 750°C (1382°F) in a vacuum furnace, which drives out any trapped hydrogen. We also advise clients to avoid prolonged exposure to acidic solutions with low pH (below 4), and if that’s unavoidable, we recommend using a titanium alloy with higher hydrogen resistance, like Ti-Pd, which has a small amount of palladium added to improve corrosion resistance and reduce hydrogen uptake. For the plating client, we switched their anode baskets to Ti-Pd, added a hydrogen monitoring probe to their plating baths, and adjusted their process to reduce hydrogen generation during operation.

Beyond these specific failure types, there are two universal causes of titanium equipment failure that every supplier and client needs to prioritize: improper installation and lack of regular maintenance. Even the best titanium design and material will fail if bolts are overtightened (creating excessive stress) or gaskets are misaligned during assembly. And while titanium is low-maintenance, that doesn’t mean no maintenance—skipping annual NDT inspections, failing to clean process lines, or ignoring small leaks can turn minor issues into major failures.

As a titanium equipment supplier, our job isn’t just to sell you high-quality components—it’s to support you from design through installation and long-term operation. We don’t just ship a titanium reactor and disappear; we provide pre-fabrication testing, on-site installation support, and annual maintenance checklists tailored to your specific process. We also offer training for your team to spot early warning signs: discoloration on the titanium surface (which can indicate oxide layer damage), unusual noise from equipment, or small leaks that signal a weakening joint.

At the end of the day, the most effective way to prevent titanium equipment failure is to partner with a supplier who understands both the science of titanium and the real-world demands of your industry. If you’re dealing with premature equipment failure, planning a new titanium installation, or just want to optimize your current setup, reach out to our team to discuss your needs. Our experts can assess your application, identify potential weak points, and provide customized solutions to keep your equipment running reliably for years to come.

Titanium Sheet References

  1. “Corrosion of Titanium and Titanium Alloys,” National Association of Corrosion Engineers (NACE) International, 2015.
  2. Stress Corrosion Cracking of Titanium Alloys, International Organization for Standardization (ISO) 10271, 2019.
  3. Titanium Equipment Design and Manufacturing Guidelines, American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code, Section VIII, Division 1, 2021.
  4. Hydrogen Embrittlement in Industrial Titanium Applications, Society for Corrosion Engineers (SCCE), 2020.
  5. Surface Roughness Standards for Titanium Components, ASTM International B265-21, 2021.

Baoji Yinnly Titanium Co., Ltd.
Baoji Yinnly Titanium Co., Ltd. is one of the most professional titanium equipment manufacturers and suppliers in China, featured by quality products and good service. Please rest assured to buy bulk titanium equipment in stock here and get quotation from our factory. Customized orders are welcome.
Address: Unit 902, Building 1, Creative Building, No. 195, Gaoxin Avenue, High-tech Zone, Baoji City, Shaanxi Province
E-mail: anna@yinnlyti.com
WebSite: https://www.yinnlyti.com/